Description:
SS-307 gives full austenite structure containing 4-5% Mn. Weld metal is highly resistant to impact, wearing and hot cracking. It is suitable for forming a buffer layer for hardfacing and joining of armour steel plates that are low hardenable and work-hardening austentic Mn steels. It can also be used for dissmilar joining C-Mn steels with austentic and ferritic stainless stells.
Applications:
Typical applications include stainless steel piping in refineneries and chemical plants.
Note On Usage:
1. Rebake the electrodes at 200° C for 1 hour and keep it at 100° C prior to use.
2. Use stainless steel wire brush for cleaning of slags.
3. Follow the recommended welding parameters to achieve good sound welds.
Typical Chemical Compotion Of Weld Metal (wt%) :
Weld Metal Analysis :
Carbon (C) 0.065
Chronium (Cr) 19.50
Nickel (Ni) 9.52
Manganese (Mn) 4.30
Silicon (Si) 0.55
Phosphorus (P) 0.010
Sulphur (S) 0.013
Molybdenum (Mo) 0.800
Typical Mechanical Properties Of Weld Metal :
TS N/mm2 610
EL% 39
Approvals And Conformances :
-
Sizes And Recommended Current Range (AC or DC <+> )
|
Diameter |
Length |
Amp |
|
mm |
mm |
F |
V&OH |
|
2.6 |
300 |
50-85 |
45-80 |
|
3.2 |
350 |
80-120 |
70-110 |
|
4.0 |
350 |
100-150 |
90-135 |
|
5.0 |
350 |
140-180 |
|
|